池底堆積物バイオ炭とフライアッシュを用いた高強度・低炭素型マグネシウムオキシサルフェートセメントの開発
Developing Sustainable Magnesium Oxysulfate Cement with Pond Sediment Biochar and Fly Ash for High Strength and Low Carbon Emissions (原題)
Qi Guo Sun, Zitong Lei, Yiyin Wang, Yi Chen, Yuxin Zhu, Rongxi Tian
🤖 gxceed AI 要約
日本語
池底堆積物バイオ炭(SBC)とフライアッシュ(FA)を組み合わせたマグネシウムオキシサルフェートセメント(MOSC)の力学特性と微細構造を系統的に検討した研究。SBC20%・FA30%の最適配合で28日曲げ強度が17%向上し、初期圧縮強度は93〜99MPaに達する。炭素足跡は最小333.16 kgCO2/m3と試算され、廃棄物活用による低炭素建設材料の可能性を示す一方、SBC40%以上では耐久性が低下する。
English
This study examines how pond sediment biochar (SBC) and fly ash (FA) synergistically affect the strength and microstructure of magnesium oxysulfate cement. An optimal mix of 20% SBC and 30% FA raised 28-day flexural strength by 17% and achieved early compressive strength of 93–99 MPa, with a carbon footprint as low as 333.16 kgCO2/m3. High SBC content (≥40%) increased porosity and reduced water resistance, showing a trade-off between waste valorization and durability.
Unofficial AI-generated summary based on the public title and abstract. Not an official translation.
📝 gxceed 編集解説 — Why this matters
日本のGX文脈において
建設資材の低炭素化はScope 3排出削減の重要領域であり、廃棄物由来原料の活用事例として日本企業の調達・サプライチェーン脱炭素の参考になりうる。ただし現段階では材料実験の域を出ず、SSBJや有報開示への直接的示唆は限定的。
In the global GX context
Embodied carbon in construction materials is a growing focus under Scope 3 accounting and green procurement frameworks such as the EU CBAM and LEED. This paper offers a waste-valorization route to lower-carbon binders, though it remains at laboratory scale with limited direct linkage to TCFD/ISSB disclosure requirements.
👥 読者別の含意
🔬研究者:廃棄物由来バイオ炭とフライアッシュの相乗効果を微細構造レベルで理解するための実験的知見を提供する。
🏢実務担当者:建設資材の調達段階で低炭素セメントの選択肢を検討する際の材料特性・炭素強度データの参考になる。
📄 Abstract(原文)
Abstract The valorization of solid wastes for low-carbon magnesium-based binders offers a promising pathway for sustainable construction materials. This study systematically investigates the synergistic effects of fly ash (FA) and pond sediment biochar (SBC) on the mechanical performance and microstructure of magnesium oxysulfate cement (MOSC). At an optimal combination of 20% SBC and 30% FA, the 28-day flexural strength increases by 17% compared with plain MOSC, while early compressive strength reaches 93–99 MPa. Microstructural analyses show that low SBC content ( ≤ 20 % ) promotes 5·1·7 phase formation and interfacial densification, whereas high-SBC content ( ≥ 40 % ) increases porosity and leaves unreacted MgO, reducing water resistance (softening coefficient below 0.85 for all mixes). Water absorption remains below 7% for all mixes. Carbon footprint analysis reveals emissions as low as 333.16 kgCO 2 / m 3 . These findings demonstrate that appropriate SBC and FA dosages can achieve high strength and low carbon emissions, while excessive SBC compromises durability.
🔗 Provenance — このレコードを発見したソース
- openalex https://doi.org/10.1061/jmcee7.mteng-25004first seen 2026-11-19 05:07:15
🔔 こうした論文の新着を逃したくない方は キーワードアラート に登録(無料・3キーワードまで)。
gxceed は公開メタデータに基づく研究支援データセットです。要約・翻訳・解説は AI 支援で生成されています。 最終的な解釈・検証は利用者が原典資料に基づいて行うことを前提とします。