PHYSICO-CHEMICAL FEATURES OF THE DECARBONIZATION PROCESS IN PORTLAND CEMENT PRODUCTION
ポルトランドセメント製造における脱炭酸プロセスの物理化学的特徴 (AI 翻訳)
Mariia Karpets, Olga Greyda
🤖 gxceed AI 要約
日本語
セメント製造の脱炭酸工程におけるNaF添加剤の効果を調査。2%添加で焼成温度を下げ、CO2排出削減に寄与する可能性を示した。
English
This study investigates the effect of NaF additive on the decarbonization process in Portland cement production. It finds that 2% NaF accelerates sintering and reduces temperature, potentially lowering CO2 emissions.
Unofficial AI-generated summary based on the public title and abstract. Not an official translation.
📝 gxceed 編集解説 — Why this matters
日本のGX文脈において
本論文はセメント製造の脱炭酸工程に焦点を当てており、日本のGX政策や開示基準との直接的な関連性は低いが、産業部門のエネルギー効率改善という観点では参考になる可能性がある。
In the global GX context
While this paper focuses on a specific industrial process, its findings could inform energy efficiency improvements in cement manufacturing globally, contributing to industrial decarbonization. However, it lacks direct relevance to climate disclosure or policy frameworks.
👥 読者別の含意
🔬研究者:For researchers in cement chemistry, the NaF additive shows potential for lowering decarbonization temperature.
🏢実務担当者:Cement producers can consider NaF as a mineralizer to reduce energy consumption and CO2 emissions.
📄 Abstract(原文)
The production of a high-quality, competitive Portland cement is one of the urgent tasks, which are necessary for the reconstruction of Ukraine in context of the deconstruction and damage of a large number of infrastructure objects. The technology of cement production is multi-stage and energy-intensive. One of the earliest and most important stages is the decarbonization, which is accompanied by the release of CO2 and formation of a mixture melt. The aim of work was to improve the decarbonization process, which is the primary stage of clinker minerals formation during sintering of the bath. We have investigated on PJSC Ivano-Frankivskcement an effect of the additive NaF (1-5%) on the raw material: limestone, marl and pyrite cinders in comparison with the model reaction. It has been proven, that sodium fluoride accelerates sintering of limestone and marl, but in the case of pyrite cinder, on the contrary, it slows down. The action of mineralizator comes down to lowering the temperature, appearance of the melt in the mixture that accelerates speed of sintering and contains crystalline quartz and limestone. Under these conditions, favorable conditions are formed for dissolution of CaO and C2S. The use of the mineralizator is recommended by calcination of raw mixtures. It has been established that NaF additive in the amount of 2% by the mass accelerates the process of interaction between CaO and SiO2, promotes the formation of aluminate and ferrite phases at lower temperatures. X-Ray analysis was conducted, proving that the use of mineralizer is expedient during raw mixture sintering. This work is important for improving Portland cement production technology by reducing the temperature of the decarbonization process through the introduction of the NaF additive.
🔗 Provenance — このレコードを発見したソース
- crossref https://doi.org/10.20998/2079-0821.2026.01.08first seen 2026-05-28 05:28:19 · last seen 2026-06-10 05:41:34
🔔 こうした論文の新着を逃したくない方は キーワードアラート に登録(無料・3キーワードまで)。
gxceed は公開メタデータに基づく研究支援データセットです。要約・翻訳・解説は AI 支援で生成されています。 最終的な解釈・検証は利用者が原典資料に基づいて行うことを前提とします。