フライアッシュ・ジオポリマー壁ブロック向け20%籾殻灰・6%アルカリ配合:壁1m2あたりの強度・コスト・炭素で価格づけした配合探索

A 20% Rice-Husk Ash, 6% Alkali Formulation for Fly-Ash Geopolymer Wall Blocks: A Formulation Search Priced in Strength, Cost and Carbon per Square Metre of Wall (原題)

William Alexander Aldred

Zenodo (CERN European Organization for Nuclear Research)📚 査読済 / ジャーナル2026-11-10#CCUS経営インパクト: コスト削減対象セクター: construction
DOI: 10.5281/zenodo.24108869
原典: https://doi.org/10.5281/zenodo.24108869

🤖 gxceed AI 要約

日本語

籾殻灰・フライアッシュ系ジオポリマー壁ブロックの配合を240通り探索したシミュレーション研究。推奨配合(籾殻灰20%、Na2O換算6%、60℃・24時間養生)で8.02MPa、壁1m2あたり17.30ドル・24.28kgCO2e。活性化剤がコストの39.3%、炭素の76.7%を占め、これが最大の削減レバーとなる。

English

A simulated search over 240 mix designs for alkali-activated fly-ash wall blocks, scored in strength, cost and embodied carbon per m2 of wall. The recommended mix (20% rice-husk ash, 6% Na2O dose, 60 C/24 h) reaches 8.02 MPa at US$17.30 and 24.28 kg CO2e per m2. The activator drives 39.3% of cost and 76.7% of carbon, making it the key decarbonization lever.

Unofficial AI-generated summary based on the public title and abstract. Not an official translation.

📝 gxceed 編集解説 — Why this matters

日本のGX文脈において

建設資材の炭素集約度を壁面積あたりで評価する視点は、Scope 3カテゴリ1(購入資材)や建築物のLCA開示を進める日本企業に示唆を与える。ただし未測定のシミュレーションであり、実用には試験データが必要。

In the global GX context

Frames embodied carbon per functional unit (m2 of wall), aligning with the direction of ISSB/CSRD Scope 3 and building LCA disclosure. However, results are simulated and unverified, so it offers methodological framing rather than deployable evidence.

👥 読者別の含意

🔬研究者:配合探索を強度・コスト・炭素の多目的で評価する枠組みと、活性化剤が支配的ボトルネックである点を参考にできる。

🏢実務担当者:建材の炭素・コストを面積あたりで比較する発想はScope 3算定や調達判断に応用可能だが、実測検証が前提。

📄 Abstract(原文)

A formulation search (SIMULATED, NOT MEASURED; nothing built or load-tested) over 240 combinations of rice-husk ash share (0-40%), activator dose (4-10% Na2O equivalent), curing temperature (23-80 C) and curing time (12-48 h) for an alkali-activated fly-ash wall block, scored in strength, cost and embodied carbon per square metre of 150 mm hollow-block wall. The recommended robust formulation - 20% rice-husk ash, 6% dose, cured 60 C for 24 h - reaches 8.02 MPa at US$17.30 and 24.28 kg CO2e per m2; the activator is 39.3% of cost and 76.7% of carbon, a 100-house programme needs 194.4 tonnes of activator bought in, and doses above 8% are excluded by a stated high-alkali handling limit.

🔗 Provenance — このレコードを発見したソース

🔔 こうした論文の新着を逃したくない方は キーワードアラート に登録(無料・3キーワードまで)。